Study on Microbial Analysis and Surface Characterization of SABIC Carbon Steel Corrosion in Soils of Different Moisture Levels
It investigated the impact of three different soil types in Saudi Arabia on specimens of SABIC carbon steel grade X60 (SCSX60). The findings showed that the environmental influence of different environments was very evident, suggesting that SCSX60 specimens were very corrosive to the soils studied. Based on the moisture content and immersion time, the composition…